First published in 1995, Surface Analysis of Paper examines surface analysis techniques from a paper industry perspective and places heavy emphasis on applications. Modern techniques, including ion mass spectrometry, infrared spectroscopy, and optical profilometry are reviewed in a straightforward manner. This new book provides details on widely used methods and instruments, and discusses how they can be used to attain, for example, contour maps of the microscopic constituents on paper surfaces and accurate analyses of the physical properties of paper.

Organized into three sections, Surface Analysis of Paper provides thorough coverage of the physical characteristics of paper, and a clear picture of new and emerging analytical methods. Carefully chosen background material on fundamental concepts is included wherever such material assists in understanding the uses of analysis methods.

Each chapter contains:

An introduction

A description of the technique

A discussion of the type of information that can be obtained with the particular technique

Practical examples to demonstrate the advantages of the technique

Læs hele beskrivelsen
Detaljer
  • SprogEngelsk
  • Sidetal356
  • Udgivelsesdato07-05-2019
  • ISBN139780367234690
  • Forlag Crc Press
  • FormatHardback
Størrelse og vægt
  • Vægt807 g
  • coffee cup img
    10 cm
    book img
    17,8 cm
    25,4 cm

    Findes i disse kategorier...

    Se andre, der handler om...

    Velkommen til Saxo – din danske boghandel

    Hos os kan du handle som gæst, Saxo-bruger eller Saxo-medlem – du bestemmer selv. Skulle du få brug for hjælp, sidder vores kundeservice-team klar ved både telefonerne og tasterne.

    Om medlemspriser hos Saxo

    For at købe bøger til medlemspris skal du være medlem af Saxo Premium, Saxo Shopping eller Saxo Ung. De første 7 dage er gratis for nye medlemmer. Medlemskabet fornyes automatisk og kan altid opsiges. Læs mere om fordelene ved vores forskellige medlemskaber her.

    Machine Name: SAXO080