This collection explores all aspects of metallurgical processing, materials behavior, and microstructural performance for the distinct class of 718-type superalloys and derivatives. Technical topics focus on alloy and process development, production, product applications, trends, and the development of advanced modeling tools. New developments in R&D, new processing methods, 3D printing, and other nontraditional applications also are covered.